Customization: | Available |
---|---|
Chemical Component: | AG and Pb |
Service Leaf: | Over 6 Years |
Still deciding? Get samples of US$ 1/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Material | Use environment | Max. Working current density(A/m2) | consumption(Kg/A.a) | Polarization potential ≤V | |
Lead silver alloy anode | Contain 20%Ag | In the seawater | 50~250 | 1×10-1 | 2.0 |
Contain 20%Ag | 50~300 | ||||
Lead silver micro-platinum anode | In the seawater | 50~1000 | 8×10-3 | 2.2 |
Chemical elements | Ag | Pb | Impurity ≤ | |
Fe | Cu | |||
Content | 2~3 | Remain | 0.005 | 0.03 |
Name | Type | Shape | Dimension (mm) | Anode body working area(mm2) | Anode body thickness(mm) | Service life | Work current range | |||
L(D) | B | H | Installation hole | |||||||
Lead silver alloy anode | YH-NPF | linear | 920 | 180 | 40 | 8 | 600×50 | 32 | >6 | 1.5~7.5 |
YH-NPF | linear | φ1340 | 180 | 40 | 10 | 1018×50 | 32 | 2.5~12.5 | ||
YH-NPF | disc | φ198 | φ146 | 25 | - | 16700 | 35 | 0.8~5.0 | ||
YH-NPF | disc | φ290 | φ245 | 30 | - | 50000 | 40 | 2.5~15 |